Amine Gold Nanorods, 25nm diameter, absorption max 650nm


Our amine terminated gold nanorods are ideal for use in applications that require conjugation of proteins or other ligand to the nanorod surface.. 

  • Description

  • Product Sheet And SDS

Amine Gold Nanorods (amine-PEG3000-SH), 25nm diameter, absorption max 650nm

Core dimensions: 60nm x 27nm

Aspect ratio: 2.2

Longitudinal peak wavelength: 650nm

Transverse peak wavelength: 518nm

Functional group: amine terminated

Linker size: 3 kDa

Zeta potential: +4 mV

Optical density: 50

Formulation: Supplied in ddH2O

Properties

Our amine terminated gold nanorods are ideal for use in applications that require conjugation of proteins or other ligand to the nanorod surface.. 

PEGylated gold nanorods are extensively purified after synthesis which reduces contaminants from manufacturing that might interfere with sensitive downstream applications.

Amine Gold Nanorods


Storage

This product should be stored at 4°C. If stored unopened and as specified, amine terminated gold nanorods are stable for at least 6 months.

55 / 100
Variable

Amine Gold Nanorods (amine-PEG3000-SH)- 10nm diameter, absorption max 770nm
Amine Gold Nanorods (amine-PEG5000-SH)- 10nm diameter, absorption max 770nm
Amine Gold Nanorods (amine-PEG3000-SH)- 15nm diameter, absorption max 700nm
Amine Gold Nanorods (amine-PEG5000-SH)- 15nm diameter, absorption max 700nm
Amine Gold Nanorods (amine-PEG3000-SH)- 25nm diameter, absorption max 650nm
Amine Gold Nanorods (amine-PEG5000-SH)- 25nm diameter, absorption max 650nm

Optimized by Optimole
>